3M 90CA
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- Fast Tack Spray Bonding
- Adjustable Lace Spray Pattern
- Broad Assembly Material Compatibility
Product Description
3M Hi-Strength 90 CA Spray Adhesive is a high-strength, fast-tacking spray contact adhesive for assembly and maintenance bonding. Its synthetic elastomer base delivers a clear adhesive layer with a variable lace spray pattern, helping users apply coverage across broad surfaces. A 1 to 4 minute dry time and a 1 to 30 minute bonding range support practical positioning before parts are joined. The low-VOC formulation is suited to regulated aerosol applications, while the adhesive bonds laminates, wood, fabrics, and many plastics when the substrate and process conditions are compatible.
Key features
- Fast Tack Development: A short dry time supports efficient assembly before parts are joined.
- Adjustable Lace Spray: The variable spray pattern helps control coverage across different work areas.
- Broad Material Compatibility: The adhesive supports bonding of laminates, wood, fabrics, and many plastics.
Applications
General assembly, maintenance bonding, laminate attachment, fabric bonding, woodworking, and compatible plastic bonding.
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Base | Synthetic elastomer | - | As supplied |
| Color | Clear | - | As supplied |
| Solids by weight | 23.2 | % | Typical |
| Density | 7.3 | lb/gal | Typical |
| Dry time | 1 to 4 | min | Before bonding |
| Bonding range | 1 to 30 | min | After spray application |
| Coverage | 50 | ft2/can | At 2.5 g/ft2 coating weight |