BONDERITE M-CR 120
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Two-Step Aluminum Deoxidizing and Coating
- Manual Brush-Applied Aluminum Treatment
- Pre-Portioned Two-Component Kit Packaging
Product Description
BONDERITE M-CR 120 Kit is a two-component, brush-applied aluminum surface-treatment kit supplied as a case of three kits, each containing one pint of BONDERITE M-CR 1201 conversion coating and one pint of BONDERITE C-IC 605 deoxidizer and cleaner. The kit pairs a deoxidizing cleaning step with a chromate conversion-coating step for sequential brush application to aluminum surfaces ahead of painting or corrosion-protection processes. Because the kit combines two separately formulated chemicals, technical and safety information should be referenced by component rather than treated as a single blended product.
Key features
- Two-Step Aluminum Treatment Process: combines deoxidizing and cleaning with chromate conversion coating in a single kit
- Manual Brush-Applied Format: both components are applied by brush for localized or touch-up treatment
- Pre-Portioned Case of Three Kits: supplied as three sets, each with one pint of BONDERITE M-CR 1201 and one pint of BONDERITE C-IC 605
Applications
Brush-applied preparation and chromate conversion coating of aluminum surfaces.