CYBERBOND 6020

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

CYBERBOND 6020

Main features

  • Targeted Cyanoacrylate Residue Removal
  • Low-Viscosity Surface Treatment
  • Repeat-Application or Soak Removal

Product Description

Cyberbond UNDO 6020 is a nitromethane-based liquid remover for softening and dissolving cyanoacrylate adhesive in unwanted areas. The colorless, low-viscosity material can be applied to residue on compatible metal, plastic, and rubber surfaces, then allowed to work for several minutes before wiping or cleaning. Heavier deposits may require repeated application, while bonded parts may require extended soaking. The product has a typical viscosity of 1 cP and a specific gravity of 1.1 g/cm^3. Some plastics and other materials may be adversely affected.

Key features

  • Cyanoacrylate residue removal: The liquid softens and dissolves unwanted cyanoacrylate adhesive.
  • Low-viscosity application: The 1 cP remover can reach residue on compatible metal, plastic, and rubber surfaces.
  • Wipe or soak processing: Removal can use several-minute treatment, repeated application, or extended soaking for bonded parts.

Applications / Suitable for

  • Removing cyanoacrylate residue from compatible metal surfaces
  • Softening cyanoacrylate on compatible plastic and rubber surfaces
  • Separating bonded parts through extended soaking where appropriate
Product Family

CYBERBOND 6020

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colorless liquid
Specific GravitySpecific Gravity
1.1
Vapor DensityVapor Density
Heavier than air
Physical Properties
ViscosityViscosity
1 mPa.s
Thermal Properties
Boiling PointBoiling Point
101 °C
Flash PointFlash Point
96 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical liquid properties for the cyanoacrylate remover; values are not specifications.

Property Value Unit Method / condition
Base compound Nitromethane Liquid
Appearance Colorless liquid As supplied
Viscosity 1 cP Typical liquid property
Specific gravity 1.1 g/cm^3 Typical liquid property
Flash point 96 deg C As supplied
Boiling point 214 deg F As supplied
Shelf life 18 months Unopened

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers