PERMABOND 2K
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- 1 mPa s Low Viscosity
- Eight-Hour Mixed Working Life
- Visible Red Coverage
Product Description
PERMABOND 2K Primer is a two-component, red liquid surface treatment for preparing metal, glass, plastic, and composite substrates before bonding with engineering adhesives. The mixed primer has a typical viscosity of 1 mPa s and specific gravity of 1.0, allowing a thin, visible coating that indicates surface coverage. Its mixed working life is 8 hours, and unopened material has a 24-month shelf life when stored at 5-25 deg C. It is used before compatible epoxy, acrylic, polyurethane, and other engineering adhesive systems; the primer itself does not form the bonded joint.
Key features
- Visible red coverage: The red liquid provides a visual indication of primer wetting and surface coverage.
- Low-viscosity application: A typical viscosity of 1 mPa s supports thin surface treatment.
- Eight-hour mixed life: The combined primer remains usable for up to 8 hours.
Applications / Suitable for
- Preparing metal and glass surfaces before adhesive bonding
- Preparing plastic and composite surfaces
- Use before compatible epoxy, acrylic, and polyurethane adhesive systems
TDS, SDS & Technical Documents
Technical Specifications
Other Properties
General Properties
Physical Properties
Thermal Properties
Additional Information
As-supplied and working properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Red liquid | Mixed primer | |
| Viscosity | 1 | mPa s | Typical |
| Specific gravity | 1.0 | Typical | |
| Flash point | 55 | deg C | Typical |
| Mixed working life | 8 | h | After combining components |
| Shelf life | 24 | months | Unopened; stored at 5-25 deg C |