PERMABOND MM115
Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

Main features
- 10-Minute Handling Strength
- Controlled Medium-Strength Off-Torque
- Serviceable Thread Locking and Sealing
Product Description
Permabond MM115 is a blue, single-part anaerobic threadlocker and sealant for metal bolts, nuts, and screws that may require service disassembly. The thixotropic methacrylate formulation cures at room temperature, reaches handling strength on M10 steel in about 10 minutes at 23 deg C, and develops full strength after 24 hours. Its medium-strength cured joint provides 16 N m breakaway torque and 7 N m prevailing torque on M10 steel under ISO 10964. Applications include machinery and equipment fastener retention where ordinary tools are required for later disassembly.
Key features
- Serviceable Medium Strength: Allows disassembly of threaded fasteners with ordinary tools.
- 10-Minute Handling: Reaches handling strength on M10 steel in about 10 minutes at 23 deg C.
- Controlled Off-Torque: Provides 16 N m breakaway and 7 N m prevailing torque on M10 steel.
Applications
Applications include locking and sealing metal bolts, nuts, and screws in machinery and equipment that may require service or maintenance disassembly.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Electrical Properties
Thermal Properties
Additional Information
As supplied / before processing
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical composition | Methacrylate esters | As supplied | |
| Appearance | Blue | As supplied | |
| Viscosity | 1,300 | mPa s | 20 rpm at 25 deg C; thixotropic |
| Specific gravity | 1.1 | As supplied | |
| Maximum gap fill | 0.15 | mm | Typical curing property |
| Handling strength | 10 | minutes | M10 steel at 23 deg C |
| Full strength | 24 | hours | M10 steel at 23 deg C |
After processing / final state
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Breakaway torque | 16 | N m | M10 steel; ISO 10964 |
| Prevailing torque | 7 | N m | M10 steel; ISO 10964 |
| Compressive shear strength | 10 | MPa | Steel collar and pin; ISO 10123 |
| Coefficient of thermal expansion | 90 x 10^-6 | mm/mm/deg C | Typical cured value |
| Dielectric strength | 11 | kV/mm | Typical cured value |
| Thermal conductivity | 0.19 | W/(m K) | Typical cured value |