PERMABOND TA4246
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- 1-2 Minute Aluminum Fixture
- 33-35 N/mm2 Steel Shear
- No-Mix Initiator 46 System
Product Description
Permabond TA4246 is a two-part, no-mix toughened acrylic structural adhesive used with Permabond Initiator 46. The adhesive is applied to one surface and the initiator to the other, eliminating premixing while supporting room-temperature assembly. It fills gaps up to 0.5 mm, fixtures aluminum in 1-2 minutes at 23 deg C, and reaches working strength in 15-30 minutes. After a 24-hour cure, typical shear strength is 33-35 N/mm2 on mild steel and 20-30 N/mm2 on aluminum, with 150-180 N/25 mm peel strength. Applications include structural bonding across supported metals, plastics, ceramics, and other substrates.
Key features
- No-Mix Structural Bonding: Separate adhesive and Initiator 46 application eliminates premixing.
- 1-2 Minute Aluminum Fixture: Fixtures gap-free aluminum in 1-2 minutes at 23 deg C.
- High Shear and Peel: Provides 33-35 N/mm2 steel shear and 150-180 N/25 mm aluminum peel strength.
Applications
Applications include structural bonding of supported metals, plastics, ceramics, wood, glass, and composite materials.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Curing Conditions
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As supplied / before processing
Resin values are shown with processing values for use with Permabond Initiator 46.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Amber liquid | As supplied | |
| Viscosity | 15,000-35,000 | mPa s | 20 rpm at 25 deg C |
| Specific gravity | 1.0 | Resin as supplied | |
| Use ratio | Approx. 10:1 | TA4246 adhesive to Initiator 46 | |
| Maximum gap fill | 0.5 | mm | Typical curing property |
| Cure milestones | Fixture: 1-2; handling: 2-4; working strength: 15-30 | minutes | Aluminum, no gap, at 23 deg C |
| Full cure | 24 | hours | At 23 deg C |
| Storage temperature | 2 to 7 | deg C | Recommended storage range |
After processing / final state
Values are typical for fully cured adhesive; strength depends on surface preparation and bond gap.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shear strength - mild steel | 33-35 | N/mm2 | ISO 4587 |
| Shear strength - aluminum | 20-30 | N/mm2 | ISO 4587 |
| Peel strength - aluminum | 150-180 | N/25 mm | ISO 4578 |
| Tensile strength | 30 | N/mm2 | ISO 37 |
| Impact strength | 50-60 | kJ/m2 | ASTM D-950 |
| Coefficient of thermal expansion | 80 x 10^-6 | 1/K | ASTM D-696 |
| Thermal conductivity | 0.1 | W/(m K) | ASTM C-177 |
| Dielectric strength | 30-50 | kV/mm | ASTM D-149 |