PLEXUS PC-120

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PLEXUS PC-120

Main features

  • Visible Red Application Indicator
  • Fast 1-3 Minute Bonding Window
  • Brush or Wipe Metal Conditioning

Product Description

Plexus PC-120 Cleaner/Conditioner is a fast-drying metal surface treatment used before bonding aluminum and stainless steel with Plexus adhesives. The chemical cleaner and conditioner is applied by brushing or wiping, then allowed to dry slightly before excess material is removed. A red dye leaves a visible tint, giving operators a direct indication that a thin film has been applied. At ambient temperature, treated parts can be bonded 1-3 minutes after application. Approximate coverage is 250 sq ft per 500 ml, making PC-120 suited to controlled metal pretreatment where long-term bond durability under demanding exposure is required.

Key features

  • Visible application indicator: A red dye leaves a slight tint that confirms a thin conditioner film is present.
  • Fast bonding window: Treated parts can be bonded 1-3 minutes after application at ambient temperature.
  • Brush or wipe application: The cleaner/conditioner can be applied by brushing or wiping, with approximately 250 sq ft coverage per 500 ml.

Applications / Suitable for

  • Cleaning and conditioning aluminum surfaces before bonding with Plexus adhesives.
  • Cleaning and conditioning stainless steel surfaces before bonding with Plexus adhesives.
Product Family

PLEXUS PC-120

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage TemperatureStorage Temperature
15 - 30 °C
General Properties
ColorColor
Translucent red dye
Density (g)Density (g)
0.977 g/cm3
SolidsSolids
5 %
SolventSolvent
Isopropyl Alcohol
Thermal Properties
Flash PointFlash Point
12.78 °C

Additional Information

Technical properties

As supplied / before processing

Application values describe the cleaner/conditioner before adhesive bonding.

Property Value Unit Method / condition
Visual indicatorRed dye-A slight red tint indicates sufficient conditioner
Application methodBrush or wipe-Apply a thin film and remove excess after slight drying
Bonding window1-3minAfter application at ambient temperature
Approximate coverage250sq ft per 500 mlTypical application coverage
Package size1 quart bottle-Supplied package format

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers