STYCAST 1265
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

Main features
- Soft-Gel Stress-Sensitive Encapsulation
- Extended 24-Hour Work Life
- Cuttable Repair Access
Product Description
LOCTITE STYCAST 1265 Epoxy Encapsulant is a clear, two-component epoxy system that cures to a soft gel for encapsulating stress-sensitive electrical and electronic components. The 100:100 by-weight mix has a typical mixed viscosity of 600 cP, a specific gravity of 1.08, and more than 24 hours of working life at 25 deg C. Its low-exotherm cure can proceed at room temperature or with heat, while the final 25 Shore A material remains cuttable for repair access and repouring. The nonconductive gel supports inspection, protection, and re-entry in delicate assemblies.
Key features
- Soft-gel encapsulation: The cured material has a typical hardness of 25 Shore A.
- Extended working time: More than 24 hours of work life supports controlled filling and assembly.
- Repair-accessible protection: The cured gel can be cut and repoured for inspection or repair.
Applications
Applications include encapsulation of stress-sensitive electrical and electronic components requiring a soft, nonconductive gel and later repair access.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Electrical Properties
Other Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Two-component clear epoxy system | Part A and Part B | |
| Mix ratio | 100:100 | parts by weight | Part A:Part B |
| Part A viscosity | 10,000 | cP | 25 deg C; typical |
| Part B viscosity | 230 | cP | 25 deg C; typical |
| Mixed viscosity | 600 | cP | 25 deg C; typical |
| Mixed specific gravity | 1.08 | 25 deg C; typical | |
| Working life | >24 | hours | 100 g mass at 25 deg C |
| Cure schedule | 3-7 d at 25 deg C; 48 h at 45 deg C; 16 h at 65 deg C; 4 h at 95 deg C | Typical options |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Operating temperature | -40 to 90 | deg C | Cured material |
| Hardness | 25 | Shore A | Typical cured value |
| Volume resistivity | 1 x 10^12 | ohm cm | 25 deg C |
| Dielectric constant | 3.0 | 1 MHz | |
| Dissipation factor | 0.02 | 1 MHz |