STYCAST 1495K
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

Main features
- Thermally Conductive Electronic Potting
- 45-Minute CAT 9 Work Life
- Transformer and Sensor Encapsulation
Product Description
LOCTITE STYCAST 1495K Thermally Conductive Epoxy Encapsulant is a black, filled epoxy encapsulant for electronic components that require a thermally conductive potting material. With CAT 9, the resin mixes 100:4.5 by weight, reaches a typical mixed viscosity of 21,000 cP, and provides a 45-minute working time at 25 deg C. The cured material has a typical thermal conductivity of 1.1 W/(m K), 95 Shore D hardness, electrical insulation, and an operating range of -40 to 130 deg C. Documented applications include transformers, sensors, and related electronic assemblies.
Key features
- Thermally conductive potting: Typical cured thermal conductivity is 1.1 W/(m K).
- Controlled CAT 9 processing: The CAT 9 formulation provides a 45-minute working time at 25 deg C.
- Electrical encapsulation: The cured material combines thermal conduction with dielectric performance.
Applications
Applications include potting of transformers, sensors, and electronic assemblies requiring a thermally conductive, electrically insulating encapsulant.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
The table uses the CAT 9 formulation; other approved catalysts have different ratios, viscosities, work lives, and cure schedules.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product form | Black filled epoxy resin | Values below use CAT 9 catalyst | |
| Resin viscosity | 45,000 | cP | Brookfield, spindle 6, 10 rpm |
| Resin specific gravity | 1.9 | Typical as supplied | |
| Mix ratio | 100:4.5 | parts by weight | Resin:CAT 9 |
| Mix ratio | 100:8.5 | parts by volume | Resin:CAT 9 |
| Mixed viscosity | 21,000 | cP | CAT 9; typical |
| Mixed specific gravity | 1.89 | CAT 9; typical | |
| Working time | 45 | minutes | CAT 9 at 25 deg C |
After-processing / final-state properties
Typical cured properties for the CAT 9 formulation.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Thermal conductivity | 1.1 | W/(m K) | CAT 9 cured formulation |
| Operating temperature | -40 to 130 | deg C | CAT 9 cured formulation |
| Hardness | 95 | Shore D | CAT 9 cured formulation |
| Linear shrinkage | 0.001 | cm/cm | CAT 9 cured formulation |
| Water absorption | 0.07 | % | 24 hours; CAT 9 cured formulation |
| Coefficient of thermal expansion | 42 | ppm/deg C | CAT 9 cured formulation |
| Dielectric strength | 15.7 | kV/mm | CAT 9 cured formulation |
| Volume resistivity | 5 x 10^13 | ohm cm | 25 deg C; CAT 9 cured formulation |